For creating coping with even wall thickness by the dipping method. Guaranteed the best fitting accuracy for the casting. Preventing accidental deformation due to high solidity of the wax, approx. 30 seconds after dipping. The dipping temperature should be between 85°C and 90°C (185°F and 195°F). With an immersion time of one second, a wall thickness of approximately 0,4 mm is achieved.
Features:
- Pure dipping wax formula
- Microcrystalline structure
- Unique elastic feel with memory
- Clean burnout with minimum shrinkage